Item Details
Quarry Location:
Mankato, Kansas
Water Absorption:
3.75 %
Density:
2480 Kg/m³
Flexural Strength:
977-987 Psi Dry
Compressive Strength:
6, 210 - 6, 420 Psi Dry
Recommended Usage:
Building stone, countertops, sinks, monuments, pool coping, sills, ornamental stone, interior, exterior, wall, floor , paving
Finishing Surface:
Honed, Aged, Polished, Sawn Cut, Sanded, Rockfaced, Sandblasted, Bushhammered, Tumbled
Additional Names:
Mankato Stone, Mankato Limestone
Description:
Testing Data:
Compressive Strength Dry, Perpendicular to Rift:6,420 PSI
Compressive Strength Dry, Parallel to Rift: 6,210 PSI
Compressive Strength Wet, Perpendicular to Rift: 5,100 PSI
Compressive Strength Wet, Parallel to Rift: 4,800 PSI
Modulus of Rupture Dry, Perpendicular to Rift: 1,029 PSI
Modulus of Rupture Dry, Parallel to Rift: 932 Psi
Modulus of Rupture Wet, Perpendicular to Rift: 910 PSI
Modulus of Rupture Wet, Parallet to Rift: 880 PSI
Flexurlal Strength Dry, Perpendicular to Rift: 987 PSI
Flexural Strength Dry, Parallel to Rift: 977 PSI
Flexural Strength Wet, Perpendicular to Rift: 717 PSI
Flexural Strength Wet, Parrallel to Rift: 710 PSI
Weight per Cubic Foot: 154 LBS/CF