No | Standard | Test Method | Result | ||
1 | ASTM C 97 | Absorption By Weight | 0.30% | ||
2 | ASTM C 99 | Modulus Of Rupture | 2000 PSI | ||
3 | ASTM C 170 | Compressive Strength | 13300 PSI | ||
4 | ASTM C 241 | Abrasion Resistance | 26.4 ha | ||
5 | ASTM C880 | Flexural Strength | 1600PSI |